BET, thermal degradation, and FTIR spectras of triazine polyamine polymers
موضوعات مرتبط
مهندسی و علوم پایه مهندسی شیمی مهندسی شیمی (عمومی)
پیش نمایش صفحه اول مقاله
BET, thermal degradation, and FTIR spectras of triazine polyamine polymers
چکیده انگلیسی

Here we show effect of the polyamine polymer chain length to BET isotherms. According to IUPAC classification [1], all three polymers are fitting type 1 physical adsorption isotherm with H3 hysteresis (except for EDA having H2 hysteresis). Moreover, TG and TGA analysis of polymers triazine-ethylenediamine (EDA) and triazine-triethylenetetramine (TETA) are provided. Due to the similarities of the structure, main decomposition temperatures are close to each other (between 593 K and 873 K). In order to understand change of FTIR spectra with adsorption and stripping Au(III), fresh, Au(III) adsorbed and recycled spectras of polymers measured. For further discussions about the effect of chain length to adsorption of Au(III) onto triazine polyamine polymer particles “Au (III) Uptake by Triazine Polyamine Polymers: Mechanism, Kinetic and Equilibrium Studies” Can et al. [2] (article in press).

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Data in Brief - Volume 11, April 2017, Pages 408-412
نویسندگان
,