Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
10155370 | Ceramics International | 2018 | 19 Pages |
Abstract
A TaSi2-MoSi2-ZrO2-borosilicate glass (TMZG) coating was prepared by a slurry method on a carbon fibre-reinforced porous silicon oxycarbide (SiCO) ceramic composite for thermal protection. The coating was well adhered to the substrate and showed a uniform thickness of approximately 375â¯Âµm. After thermal cycling from 1873â¯K to room temperature six times (total oxidation time of 180â¯min), the shape and dimension of the TMZG remain almost unchanged with no cracking or peeling of the coating surface. The TMZG-coated sample exhibits good oxidation resistance because of a molten SiO2 film with ZrSiO4 particles distributed on the outer layer of the coating. After ablation testing under an oxyacetylene flame at 1927â¯K for 90â¯s, the linear ablation rate of the TMZG coated sample are 8.33â¯Ãâ¯10â4 mm/s. The whole coating retains integrity, preventing substrate ablation during the test. The TMZG coating with excellent temperature resistance shows broad applicability in thermal insulation materials.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Xiafei Li, Junzong Feng, Yonggang Jiang, Hao Lin, Jian Feng,