In the large-scale experiment no problems were observed during the production. The bricks produced with spent grains possessed a comparable or higher strength, a higher porosity and a reduced density after firing than those from a standard production clay. Because of the lower sintering temperatures the fired clay product was more strongly sintered, exhibiting both greater strength and higher porosity.