⺠Maximum ca. 12% cellulose was dissolved in FeTNa at â9 °C under shear force. ⺠Cellulose/FeTNa solutions show gel properties measured by dynamic rheometer. ⺠In reaction calorimetry, thermal activity of solutions occurred above 80 °C. ⺠Above 90 °C decomposition of cellulose/FeTNa complex changed the color of solution.