Abstract
The 28-day compressive strength of WPLAC with the replacement ratio of 75% reduces about 33% compared to the control concrete in the water-cement ratio of 45%. The density of WPLAC varies from 1940 to 2260 kg/m3 by the influence of WPLA. The structural efficiency of WPLAC decreases as the replacement ratio increases. The workability of concrete with 75% WPLA improves about 123% compared to that of the normal concrete in the water-cement ratio of 53%. The adhered GBFS is able to strengthen the surface of WPLA and to narrow the transition zone owing to the reaction with calcium hydroxide.