The selected composition was 20% of lignite, 15% of Alumina and 65% of Kaolin, the membranes have been obtained at 1200 °C as a sintering temperature. The membranes show good behavior for both configurations, with a porosity above 36% and a mechanical strength of 39 MPa or the tubular membranes and 34% for the flat ones.