Article ID Journal Published Year Pages File Type
10625592 Ceramics International 2013 7 Pages PDF
Abstract
Combustion joining of carbon/carbon (C/C) composites using a mixture of titanium and mechanically activated Ni/Al powders as a reactive medium is reported. A minimum preheating of the sample stack to 630 K is required to initiate the joining process. A robust crack- and pore-free joint layer (∼75−100 μm in thickness), which is composed of NiAlx and TiCy(Oz) phases, is produced. Tensile-strength testing of the joined C/C composites shows that the fracture does not occur along the joint layer.
Related Topics
Physical Sciences and Engineering Materials Science Ceramics and Composites