Abstract
MAX solid solutions (Ti,V)2AlC and (Cr,V)2AlC with Al2O3 addition were produced by solid state combustion involving aluminothermic reduction in the mode of self-propagating high-temperature synthesis (SHS). Starting materials included TiO2/V2O5/Al/Al4C3 and Cr2O3/V2O5/Al/Al4C3 powder mixtures. Attempts were made to attain (Ti1−xVx)2AlC and (Cr1−yVy)2AlC with the V content in terms of x and y from 0.1 to 0.7. Combustion exothermicity was increased by increasing V2O5 for the yield of a higher proportion of V at the substitution site, which not only increased the combustion temperature and reaction front velocity, but also facilitated the evolution of solid solutions. Due to insufficient reaction exothermicity, (Ti1−xVx)2AlC/Al2O3 in situ composites were only produced under x≥0.4. On the other hand, the formation of (Cr1−yVy)2AlC/Al2O3 was achieved with y from 0.1 to 0.7, because reduction of Cr2O3 is more energetic than that of TiO2. The laminated microstructure characteristic of the MAX ternary carbide was observed for both Al2O3-added (Ti,V)2AlC and (Cr,V)2AlC composites synthesized in this study.
Related Topics
Physical Sciences and Engineering Materials Science Ceramics and Composites
Authors
, ,