The preparation and dielectric properties of 3ZnO·B2O3 ceramics were investigated. Dense 3ZnO·B2O3 ceramics were obtained as sintered in the temperature range from 950 to 1000 °C for 3 h. The X-ray diffraction showed that the obtained ceramics were of a monoclinic 3ZnO·B2O3 structure. The ceramic specimens fired at 955 °C for 1 h exhibited excellent microwave dielectric properties: ɛr ∼ 6.9, Q × f ∼ 20,647 GHz (@6.35 GHz), and τf ∼ −80 ppm/°C. The dependences of relative density, ɛr, and Q × f of ceramics sintered at 955 °C on sintering soaking time showed that they all reached their plateaus as the soaking time was up to 60 min. Meanwhile, 3ZnO·B2O3 ceramics had no reaction with silver during cofiring, indicating it is a potential candidate for low-temperature cofired ceramic (LTCC) substrate.