Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
10629760 | Journal of the European Ceramic Society | 2011 | 7 Pages |
Abstract
The refractories currently used in frit furnaces are Al2O3-ZrO2-SiO2 (AZS) fused cast materials and Cr2O3-based materials. In this work, results on dynamic corrosion studies of AZS and Cr2O3-based materials by two ZnO-containing frits are described. Experiments have been performed using the “Merry Go Round” test at â
1500 °C. Macroscopic results are analysed in terms of the remaining volume after the tests, as usually done in the glass industry. The significance and limits of such an approach are discussed.