Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
10634269 | Scripta Materialia | 2005 | 6 Pages |
Abstract
Thermal stability of PM Al/5%NiAl composites has been studied by exposure at 500 °C up to 24 h. NiAl intermetallic particles were employed as-received and after pre-oxidation at several temperatures. The optimal oxidation condition was determined based on its ability to delay interfacial reactions and prevent debonding at the metal/reinforcement interface.
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
H.A. Pour, M. Lieblich, S.G. Shabestari, M.T. Salehi,