Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
10634298 | Scripta Materialia | 2005 | 6 Pages |
Abstract
Laser deposition of Inconel 738 on directionally solidified (DS) Ni-based superalloy demonstrates a strong susceptibility to cracking. Cracks originate from the liquation of low melting point eutectic on the DS grain boundary. Five boundary liquation and interface cracking styles were identified. Sound Inconel 738 deposition layers were achieved free of cracks.