Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
10635096 | Scripta Materialia | 2005 | 9 Pages |
Abstract
The grain size of as-cast Ti-6Al-4V is reduced by about an order of magnitude from 1700 to 200 μm with an addition of 0.1 wt.% boron. A much weaker dependence of reduction in grain size is obtained for boron additions from >0.1% to 1.0%. Similar trends were observed in boron-modified as-cast Ti-6Al-2Sn-4Zr-2Mo-0.1Si.
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
S. Tamirisakandala, R.B. Bhat, J.S. Tiley, D.B. Miracle,