Article ID Journal Published Year Pages File Type
10645689 Materials Characterization 2011 6 Pages PDF
Abstract
► The Ni-CeO2 nanocomposite has been produced by a high energy ball milling technique. ► The crystallite size of Ni decreases up to a critical temperature of 45 °C and beyond this bath temperature the crystalline size of Ni again increases. ► The hardness of the nanocomposite coating increases with the increase of a bath temperature of 45 °C.
Related Topics
Physical Sciences and Engineering Materials Science Materials Science (General)