Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
10653234 | Solid State Communications | 2005 | 4 Pages |
Abstract
Sb3+-doped, Eu3+-doped and (Sb3+, Eu3+) co-doped YBO3 crystals have been synthesized using Y2O3, B2O3, SbCl3 and Eu2O3 as raw materials through a hydrothermal method. Phase-pure YBO3 crystal with hexagonal flake shape has been synthesized at 473Â K for 3 days. The photoluminescent property of YBO3 with different activators were investigated using luminescent spectrometer at room temperature. The color of the (Sb3+, Eu3+) co-doped YBO3 crystal could be controlled from blue to red by changing the Sb3+/Eu3+ ratio in the initial reactants. The nearly white emission could be obtained through changing the Sb3+/Eu3+ ratio in reaction.
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Science (General)
Authors
Fushan Wen, Wenlian Li, Ze Liu, Taeun Kim, Kiyoung Yoo, Sanghoon Shin, Jong-Ha Moon, Jin Hyeok Kim,