⺠Five types of splat morphology were identified for flame sprayed Nd-Fe-B. ⺠Standoff distances affect splat size and morphology. ⺠Phase separation by metastable phase formation and non-equilibrium solidification. ⺠Coatings have poor cohesion where they failed to build up beyond 50 μm.