Abstract
In the present study, cold-rolled low-carbon steel is annealed at three different conditions: 700â¯Â°C for 0â¯s, 800â¯Â°C for 0â¯s and 800â¯Â°C for 2â¯min at the heating rate of ~10â¯Â°C/s. Recrystallization behaviour on sample surface is studied using a heated stage Scanning Electron Microscopy and Electron Backscattered Diffraction. For the lower annealing temperature of 700â¯Â°C with no dwell, almost no recrystallization is observed and microstructure resembles the as-received deformed material with the exception of occasional sub-micron sized nuclei. For the annealing conditions of 800â¯Â°C 0â¯s and 800â¯Â°C 2â¯min, onset and evolution of recrystallization is observed in-situ as a function of the initial as-cold rolled texture. Slower recovery rate of alpha fibre than gamma fibre is observed and confirmed by lower drop in average geometrically necessary dislocation (GND) density for un-recrystallized alpha fibres (1.1E+14â¯mâ2 for 700â¯Â°C 0â¯s, 1.4E+14â¯mâ2 for 800â¯Â°C 0â¯s and 4.5E+14â¯mâ2 for 800â¯Â°C 2â¯min) than for un-recrystallized gamma fibre grains (3.0E+14â¯mâ2 for 700â¯Â°C 0â¯s, 6.2E+14â¯mâ2 for 800â¯Â°C 0â¯s and 9.8E+14â¯mâ2 for 800â¯Â°C 2â¯min) during annealing. Strong gamma texture in recrystallized matrix is found for annealing conditions of 800â¯Â°C 0â¯s and 800â¯Â°C 2â¯min. From TEM characterisation it was shown that sub-grain boundaries are decorated with fine precipitates (diameter dâ¯<â¯15â¯nm) of titaniumâvanadium carbides (Ti,V)C for the annealing condition of 700â¯Â°C 0â¯s, which suggests that these precipitates play a major overall role in retardation of the recrystallization kinetics.
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Science (General)
Authors
Ishwar Kapoor, Yongjun Lan, Arjan Rijkenberg, Zushu Li, Vit Janik,