By synthesizing reactive powders via a self-sustaining combustion synthesis, the glycine-nitrate process, the gadolinium-doped ceria (GDC) with the chemical formula Ce0.8Gd0.2O1.9 was prepared. The resultant powders were dispersed with the terpineol as the dispersant through different methods such as ball milling and high-shear dispersing. Coagulation factor (CF) was used to mark the degree of agglomeration on the nano-scale GDC in this work. The effect of agglomeration on the densification behavior at different sintering temperatures was investigated. The studies indicated that agglomeration retarded the densification at the sintering stage. The powders with better dispersion exhibited a higher sintered density at the same temperature. After effective dispersion treatment, GDC could be fully densified at the sintering temperature of 1300 °C. The densification temperature was significantly lower than those reported previously. The high sintering kinetics of the ceramics was obtained based on the agglomeration control.

Related Topics
Physical Sciences and Engineering Chemistry Chemistry (General)