Article ID Journal Published Year Pages File Type
1265665 Ultrasonics Sonochemistry 2016 6 Pages PDF
Abstract

In this paper, 6061 aluminum alloys were soldered without a flux by the ultrasonic semi-solid coating soldering at a low temperature. According to the analyses, it could be obtained that the following results. The effect of ultrasound on the coating which promoted processes of metallurgical reaction between the components of the solder and 6061 aluminum alloys due to the thermal effect. Al2Zn3 was obtained near the interface. When the solder was in semi-solid state, the connection was completed. Ultimately, the interlayer mainly composed of three kinds of microstructure zones: α-Pb solid solution phases, β-Sn phases and Sn–Pb eutectic phases. The strength of the joints was improved significantly with the minimum shear strength approaching 101 MPa.

Related Topics
Physical Sciences and Engineering Chemistry Chemistry (General)
Authors
, , ,