Article ID Journal Published Year Pages File Type
1296965 Solid State Ionics 2008 4 Pages PDF
Abstract

The glassy and glassy-crystalline materials of nominal composition xAgI·(100-x) (0.75Ag2O·0.25P2O5), for 50 ≤ x ≤ 85, were investigated by DSC and XRD methods.For a composition corresponding to x = 50 an additional series of DSC scans at different heating rates from 6 to 20 K·min− 1 was carried out. These measurements revealed the occurrence of three crystallization processes. The systematic shifts of their characteristic temperatures, depending on the heating rates were analyzed using the Kissinger approach. Activation energies of these processes were determined. Their values are 179 kJ/mol, 156 kJ/mol and 169 kJ/mol, respectively.

Related Topics
Physical Sciences and Engineering Chemistry Electrochemistry
Authors
, , , , ,