Abstract

The preparation of cadmium sulfide nanoparticles that have a moderate pore size is reported. This preparation method involves a hydrothermal process that produces a precursor mixture and a following acid treatment of the precursor to get the porous material. The majority of the particles have a pore size close to 20 nm, which complements and fills in the gap between the existing cadmium sulfide materials, which usually have a pore size either less than 10 nm or are well above 100 nm.

Graphical abstractThe preparation involves a hydrothermal process and a subsequent acid treatment process, the majority of the particles have a moderate pore size, which complements and fills the gap between existing porous materials usually have a pore size either less than 10 nm or well above 100 nm.ZnCl2+NaOH+NaHS·xH2O⟶HydrothermalprocessCdCl2Zn5(OH)5Cl2·H2O/Cd7.23Zn2.7S10+ZnO/Cd7.23Zn2.7S10⟶DiluteHClPorousCdSFigure optionsDownload full-size imageDownload as PowerPoint slide

Related Topics
Physical Sciences and Engineering Chemistry Inorganic Chemistry
Authors
, , , , ,