Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1420639 | Dental Materials | 2015 | 10 Pages |
Abstract
hard machining and glaze firing reduced the leucite ceramic strength, while hydrofluoric acid etching did not affect the strength. Variability in the roughness might be expected after machining, since it was influenced by the machining order and by the bur pairing.
Related Topics
Physical Sciences and Engineering
Materials Science
Biomaterials
Authors
Sara Fraga, Luiz F. Valandro, Marco A. Bottino, Liliana G. May,