Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
143928 | Advanced Powder Technology | 2016 | 9 Pages |
•Waste coffee grounds were activated by KOH at various pyrolysis temperatures.•The specific capacitances are 175 F g−1 at 1 A g−1 and 475 F g−1 at 0.1 A g−1.•The power density is 7500 W kg−1 with an operating potential of 1.5 V.
Waste coffee grounds were activated by KOH at various pyrolysis temperatures, changing the ratio of the area of the mesoporous structure to that of the microporous structure, the surface area, the amount of oxygen and nitrogen functional groups in the grounds, and their chemical structure. At a pyrolysis temperature of 700 °C, the KOH-activated waste coffee grounds had a specific capacitance of 175 F g−1 at 1 A g−1 and 475 F g−1 at 0.1 A g−1 from the discharge profiles. Assembling the KOH-activated waste coffee grounds in a coin cell yielded an energy density and power density of 11 W h kg−1 and 7500 W kg−1, respectively, with an operating potential of 1.5 V, making waste coffee grounds a viable feedstock for manufacturing energy materials.
Graphical abstractFigure optionsDownload full-size imageDownload as PowerPoint slide