Abstract

Cobalt oxide was prepared from spent lithium ion batteries (LIBs) by reductive leaching, copper sulfide precipitation, cobalt oxalate precipitation and thermal decomposition. The cobalt rich non-magnetic −16 mesh fraction obtained from spent LIBs by mechanical separation was leached using 2 M H2SO4, 6 vol% H2O2, reaction temperature 60 °C, agitation speed 300 rpm, pulp density 100 g/L, reaction time 1 h. The leaching efficiency of cobalt was more than 99% and its concentration was 27.4 g/L. Copper was removed (99.9%) as CuS by precipitating with Na2S. The crystalline solid CoC2O4·2H2O selectively precipitated by treating the copper-free liquor with oxalic acid was calcined to produce crystalline Co3O4, of which primary average particle size was 340 nm.