(Ni,Mn,Co)O4 nanopowders with single cubic phase were successfully synthesized using combustion methods. Particle size of the as-burnt nanopowders after combustion was about 20 nm. Crystallization behavior of the NMC was investigated using various techniques such as X-ray diffraction (XRD), thermogravimetric (TG), Fourier transform infrared (FT-IR) spectroscopy, and transmission electron microscopy (TEM). Calcination at different temperature from 400 °C to 700 °C provides the powders with increased crystallinity and grain size. However, further increasing temperature above 800 °C for calcination, cubic spinel phase of NMC partly transformed to tetragonal spinel phase, which implies that cubic spinel phase of NMC nanopowder synthesized by combustion method becomes unstable above 800 °C.