Article ID Journal Published Year Pages File Type
1459160 Ceramics International 2016 8 Pages PDF
Abstract

High optical quality Y2O3 transparent ceramics with fine grain size were successfully fabricated by air pre-sintering at various temperature ranging from 1500 to 1600 °C combined with a post-hot-isostatic pressing (HIP) treatment using co-precipitated powders as the starting material. The fully dense Y2O3 transparent ceramic with highest transparency was obtained by pre-sintered at 1550 °C for 4 h in air and post-HIPed at 1600 °C for 3 h (the pressure of HIP 200 MPa), and it had fine microstructure and the average grain size was 0.96 μm. In addition, the in-line transmittance of the ceramic reached 81.7% at 1064 nm (1 mm thickness). By this approach, the transparent Y2O3 ceramics with fine grain size (<1.6 μm) were elaborated without any sintering aid.

Related Topics
Physical Sciences and Engineering Materials Science Ceramics and Composites