Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1462010 | Ceramics International | 2012 | 4 Pages |
Abstract
In present work, a simple and direct method was proposed, which could be applied for quantitatively calculating the percentage of 90° domain reorientation in the tetragonal phase of KNNLN ceramics. The relationship between 90° domain reorientation and poling field was established through the X-ray diffraction analysis. Experimental results indicate that the poling field of 5 kV/mm is sufficient for the reorientation of 90° domain and while the percentage of 90° domain reorientation 37.9% and piezoelectric constant 232 pC/N are obtained. The general trend of piezoelectric properties corresponds well with that of the percentage of 90° domain reorientation.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Yongjie Zhao, Yuzhen Zhao, Rongxia Huang, Rongzheng Liu, Heping Zhou,