Article ID Journal Published Year Pages File Type
1462974 Ceramics International 2011 7 Pages PDF
Abstract

65.9Cu–24.4Ti–9.7TiB2 (wt.%) composite filler was used to join Al2O3 and Ti–6Al–4V alloy. 30 vol.% TiB whiskers were in situ synthesized as reinforcements in joints. Brazing temperature was 890 °C, 910 °C, 930 °C, 950 °C and 970 °C, and the holding time was 0, 5, 10, 20, and 30 min. The microstructure and mechanical properties of brazed joints were analyzed by scanning electron microscope equipped with energy dispersive spectrometer, shear test and nano-indentation test. Results show that reaction layer Ti4(Cu,Al)2O forms at Al2O3/brazing alloy interface. The reaction between TiB2 powders and Ti atoms in brazing alloy brings on in situ synthesizing TiB whiskers in (Ti,Al)2Cu and AlCu2Ti intermetallics. Formation of TiB whiskers minimizes the mismatch of thermal expansion coefficient between Al2O3 and brazing alloy, and makes the ductile–rigid–ductile multiple layer present in joints, which reduces residual stress of joints. The maximum shear strength of joints can reach 143.3 MPa when the brazing temperature is 930 °C, and holding time is 10 min.

Related Topics
Physical Sciences and Engineering Materials Science Ceramics and Composites
Authors
, , , ,