Article ID Journal Published Year Pages File Type
1463744 Ceramics International 2012 4 Pages PDF
Abstract

Lead-free (Ba0.85Ca0.15)(Ti0.9Zr0.1)O3–x%CeO2(BCZT–xCe) piezoelectric ceramics have been prepared by the traditional ceramic process and the effects of CeO2 addition on their phase structure and piezoelectric properties have been studied. The addition of CeO2 significantly improves the sinterability of BCZT ceramics which results in a reduction of sintering temperature from 1540 °C to 1350 °C without sacrificing the high piezoelectric properties. X-ray diffraction data show that CeO2 diffuses into the lattice of BCZT and a pure perovskite phase is formed. SEM images indicate that a small addition of CeO2 greatly affects the microstructure. Main piezoelectric parameters are optimized at around x = 0.04 wt% with a high piezoelectric coefficient (d33 = 600 pC/N), a planar electromechanical coefficient (kp = 51%), a high dielectric constant (ɛr = 4843) and a low dissipation factor (tan δ = 0.012) at 1 kHz, which indicates that the BCZT–xCe ceramics are promising for lead-free practical applications.

Related Topics
Physical Sciences and Engineering Materials Science Ceramics and Composites
Authors
, , , , , , , ,