Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1471218 | Corrosion Science | 2009 | 10 Pages |
Abstract
The corrosion resistance of Ti and Ti–6Al–4V was investigated through electrochemical impedance spectroscopy, EIS, potentiodynamic polarisation curves and UV–Vis spectrophotometry. The tests were done in Hank solution at 25 °C and 37 °C. The EIS measurements were done at the open circuit potential at specific immersion times. An increase of the resistance as a function of the immersion time was observed, for Ti (at 25 °C and 37 °C), and for Ti–6Al–4V (at 25 °C), which was interpreted as the formation and growth of a passive film on the metallic surfaces.
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
V.A. Alves, R.Q. Reis, I.C.B. Santos, D.G. Souza, T. de F. Gonçalves, M.A. Pereira-da-Silva, A. Rossi, L.A. da Silva,