Abstract

The adoption of two-shifting in coal-fired power generation (switching from on-load to off-load conditions on a daily basis and off-load for the weekend) results in regular cycling of the solution chemistry of the condensed steam on the turbine discs. A first stage investigation has been made of the effect of such chemistry cycling on the corrosion potential of the disc steel. The corrosion potential is typically about +0.05 V (SCE) in off-load chemistry (aerated pure water) and below −0.6 V (SCE) in on-load chemistry (deaerated solution containing chloride or chloride and sulphate anions). The critical observation was the sluggish response of the corrosion potential upon restoration of deaerated on-load conditions with the implication of a likely increase in pit and stress corrosion crack development.