Abstract

A rotating magnetic field was used to fabricate c-axis oriented zinc oxide. The influence of rotating speed on orientation structure was also examined. The aligned axes had the largest diamagnetic susceptibility, which axis was difficult to align with a static magnetic field. In c-axis oriented ZnO, the degree of orientation (Lotgering factor) in the green compact ranged from 0.2 to 0.5 along c-axis. The Lotgering factor increased with rotating speed. For all samples with the rotating magnetic field, the degrees of orientation increased up to above 0.9 after sintering at 1573 K.