1476255 Journal of the European Ceramic Society 2010 8 Pages PDF
Abstract

ZrB2–SiC–BN ceramics were fabricated by hot-pressing under argon at 1800 °C and 23 MPa pressure. The microstructure, mechanical and oxidation resistance properties of the composite were investigated. The flexural strength and fracture toughness of ZrB2–SiC–BN (40 vol%ZrB2–25 vol%SiC–35 vol%BN) composite were 378 MPa and 4.1 MPa m1/2, respectively. The former increased by 34% and the latter decreased by 15% compared to those of the conventional ZrB2–SiC (80 vol%ZrB2–20 vol%SiC). Noticeably, the hardness decreased tremendously by about 67% and the machinability improved noticeably compared to the relative property of the ZrB2–SiC ceramic. The anisothermal and isothermal oxidation behaviors of ZrB2–SiC–BN composites from 1100 to 1500 °C in air atmosphere showed that the weight gain of the 80 vol%ZrB2–20 vol%SiC and 43.1 vol%ZrB2–26.9 vol%SiC–30 vol%BN composites after oxidation at 1500 °C for 5 h were 0.0714 and 0.0268 g/cm2, respectively, which indicates that the addition of the BN enhances oxidation resistance of ZrB2–SiC composite. The improved oxidation resistance is attributed to the formation of ample liquid borosilicate film below 1300 °C and a compact film of zirconium silicate above 1300 °C. The formed borosilicate and zirconium silicate on the surface of ZrB2–SiC–BN ceramics act as an effective barriers for further diffusion of oxygen into the fresh interface of ZrB2–SiC–BN.

Related Topics
Physical Sciences and Engineering Materials Science Ceramics and Composites
Authors
, ,