Article ID Journal Published Year Pages File Type
1477096 Journal of the European Ceramic Society 2009 5 Pages PDF
Abstract

Commercial alumina powder was densified by spark plasma sintering (SPS) at 1150 °C. During SPS processing, the effects of the heating rate were examined on microstructure and transparency. With decreasing heating rate, the grain size and the residual porosity decreased, while the transparency increased. At a heating rate of 2 °C/min, the grain size was 0.29 μm, and the in-line transmission was 46% for a wavelength of 640 nm. The mechanisms for the fine microstructure and low porosity at slow heating, which are conflicting with some existing results, were explained by considering the role of defect concentration and grain-boundary diffusion during densification.