Patterned barium strontium titanate (BST) thick films are fabricated in the grooved silicon substrate using tape casting method and sintered from 800 to 1250 °C for 2 h. The slurry used for the tape casting is from sol-precipitation method, and the crystallization of the as precipitated BST powders is improved by hydrothermal treatment at 200 °C for 5 h. The patterned BST thick films have a size of 800 × 300 μm and homogeneous thickness of 30 μm. After sintering below 1000 °C, the obtained BST thick films have a dielectric abnormality at about 30 °C and the dielectric loss is about 0.02.