Article ID Journal Published Year Pages File Type
1496122 Optical Materials 2009 6 Pages PDF
Abstract

The detailed preparation process of Eu2+ and Dy3+ ion co-doped Sr3Al2O6 phosphor powders with red long afterglow by sol–gel-combustion method in the reducing atmosphere is reported. X-ray diffraction, scanning electron microscopy and photoluminescence spectroscopy are used to investigate the effects of synthesis temperature on the crystal characteristics, morphology and luminescent properties of the as-synthesized Sr3Al2O6:Eu2+, Dy3+ phosphors. The results reveal that Sr3Al2O6 crystallizes completely when the combustion ash is sintered at 1200 °C. The excitation and the emission spectra indicate that the excitation broad-band lies chiefly in visible range and the phosphor powders emit strong light at 618 nm under the excitation of 472 nm. The light intensity and the light-lasting time of Sr3Al2O6:Eu2+, Dy3+ phosphors are increased when increasing the calcination temperatures from 1050 to 1200 °C. The afterglow of Sr3Al2O6:Eu2+, Dy3+ phosphors sintered at 1200 °C lasts for over 600 s when the excited source is cut off. The red emission mechanism is discussed according to the effect of nephelauxetic and crystal field on the 4f65d1 → 4f7 transition of the Eu2+ ions.

Related Topics
Physical Sciences and Engineering Materials Science Ceramics and Composites
Authors
, , ,