Abstract
Ge, GeO2 and Ge2C6H10O7 additions to MgB2 obtained by ex situ spark plasma sintering significantly enhance the critical current density Jc in high magnetic fields. A Jc(T = 20 K) of 102 A cm−2 is obtained at 3.9 T in the pristine sample and at 5.8 T in the MgB2(Ge2C6H10O7)0.0014 sample. The decrease in the critical temperature for added samples is less than 1 K and Jc(20 K, H = 0) shows a small decrease from 5.5 × 105 A cm−2 in the pristine sample to 3.9 × 105 A cm−2 in MgB2(Ge2C6H10O7)0.0014 sample. Ge does not substitute into the MgB2 lattice.