Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1501513 | Scripta Materialia | 2009 | 4 Pages |
Abstract
α/β Si3N4 composites were prepared by spark plasma sintering at 1340–1500 °C for 3–12 min with MgSiN2 as additives. The hardest α/β Si3N4 composite has a Vickers indentation hardness of 21.4 GPa, which is as hard as α-Sialon ceramics and harder than ordinary β-Si3N4 ceramics. The fracture toughness increased from 5.7 to 7.7 MPa m1/2 with the β-Si3N4 content increasing from 21 to 76 wt.%, and the Vickers indentation hardness of the latter was 19.0 GPa.
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Gui-hua Peng, Xiang-guo Li, Min Liang, Zhen-hua Liang, Qian Liu, Wen-lan Li,