Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1502412 | Scripta Materialia | 2006 | 4 Pages |
Abstract
The Mg–Zn–Al alloy processed by hot extrusion typically exhibits strong grain size dependence of yield stress. However, the same friction stir processed Mg–Zn–Al alloy samples exhibited much weaker grain size dependence. The high Schmid factor of around 0.3 of the friction stir processed samples is responsible for the low parameters in the Hall–Petch relationship.
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Y.N. Wang, C.I. Chang, C.J. Lee, H.K. Lin, J.C. Huang,