The eutectic silicon in A356 alloy can be refined and modified using either chemical, quench, or superheating modification. We observed, for the first time, that the eutectic silicon can also be significantly refined using high-intensity ultrasonic vibration. Rosette-like eutectic silicon is formed during solidification of specimen treated with high-intensity ultrasonic vibration.