Mesoporous α-Fe2O3-pillared titanate nanocomposites have been successfully synthesized through an exfoliation−restacking route. Powder X-ray diffraction and N2 adsorption–desorption isotherms revealed that the α-Fe2O3 pillared titanate has an interlayer distance of 3.27 nm, a specific surface area of 66 m2/g and an average pore size of 7.6 nm, suggesting the formation of a mesoporous pillared structure. UV–vis diffuse reflectance spectra show a red shift, indicative of a narrow band gap energy of ∼2.1 eV compared to the host layered titanate, which is essential in creating a visible light photocatalytic activity. The results of degradation of rhodamine B reveal that the present pillared mesoporous composites exhibit better photocatalytic activities than those of the pristine materials under visible irradiation, based on the band gap excitement and the dye-sensitized path, originated from their high surface area, mesoporosity and the electronic coupling between the host and the guest components.

Related Topics
Physical Sciences and Engineering Materials Science Electronic, Optical and Magnetic Materials
Authors
, , , , , ,