Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1524428 | Materials Chemistry and Physics | 2010 | 5 Pages |
Abstract
Nano-sized silver powders were directly prepared by high-temperature flame spray pyrolysis; an ultrasonic spray generator was used in the process. The silver powders were nanometer sized and had a spherical shape; further, they did not show a tendency to form aggregates. Their mean size was 26 nm. The mean crystallite size measured using Scherrer's equation was 26 nm. Conductive silver films were formed from the nano-sized silver powders. The powders sintered completely at a firing temperature of 400 °C. Conductive silver films fired at temperatures between 400 and 500 °C had a dense structure and similar thicknesses. The specific resistances of conductive silver films fired at temperatures of 400, 450, and 500 °C were 8.3, 3.6, and 2.7 μΩ cm. On the other hand, a conductive silver film formed from submicron-sized silver powders had a high specific resistance of 19 μΩ cm at a firing temperature of 450 °C.
Related Topics
Physical Sciences and Engineering
Materials Science
Electronic, Optical and Magnetic Materials
Authors
Hye Young Koo, Jang Heui Yi, Jung Hyun Kim, You Na Ko, Dae Soo Jung, Yun Chan Kang, Jong-Heun Lee,