Article ID Journal Published Year Pages File Type
1527809 Materials Chemistry and Physics 2006 7 Pages PDF
Abstract

Co-doped alumina powders were synthesized by means of the polymeric precursor method to obtain ceramic pigments. The effect of different contents of Co2+ on phase transition γ to α-Al2O3 and appearing of CoAl2O4 spinel were studied by means of X-ray diffraction. A partial phase diagram of the system CoAl2O3 was proposed from these data by means of determination of the percentages of these phases according to the calcining temperature. Critical particle size to phase transition was determined by means of calculations of crystallite size and determination of superficial area through the BET method. UV–vis spectroscopy of the samples allow to compare the band shift with the phase transition. Besides, a study of thermal stability and intensity of the blue coloration of the synthesized powders with the presence of cobalt in relation to the calcining temperature was accomplished and compared to the phase transition. The results show that the higher blue color intensity was obtained for the powders with Co-doped γ-Al2O3 closest of phase transition to α-Al2O3+CoAl2O4Al2O3+CoAl2O4.

Related Topics
Physical Sciences and Engineering Materials Science Electronic, Optical and Magnetic Materials
Authors
, , , , , ,