1528027 | Materials Chemistry and Physics | 2006 | 6 Pages |
Abstract
Differential scanning calorimetric (DSC) measurements have been made in glassy Se70Te30âxAgx alloys. At low concentration of Ag (x = 2, 4, 6), only one endothermic and one exothermic peaks are observed at glass transition and crystallization temperatures. However, at higher concentration of Ag (x = 8, 10), two endothermic and two exothermic peaks have been observed in DSC scans. The double stage crystallization at higher concentration of Ag has also been reported in various other glassy systems by other workers. The activation energy of crystallization (Ec) has been determined for each stage.