Article ID Journal Published Year Pages File Type
1529915 Materials Science and Engineering: B 2011 5 Pages PDF
Abstract

Continuous SiC fibers with different thickness of carbon layer were prepared through three preceramic polymer pyrolysis routes. To make the carbon layer thickness controllable, a simple improvement by using a ceramic bushing was adopted to retard the deposition of the pyrolytic carbons. Auger electron spectroscopy (AES) analysis reveals that the carbon layer thickness varies from less than 5 nm to 40 nm. The specific resistivity of the fibers increases by 5 orders of magnitude as the carbon layer thickness decreases. All of the fibers exhibit a tensile strength of around 1.8 GPa which is independent of the carbon layer thickness. The formation process of the carbon layer is discussed in three steps: the decomposition, the carbonization and the deposition. The as-received fibers have a potential application as the reinforcement of functional materials.

Related Topics
Physical Sciences and Engineering Materials Science Electronic, Optical and Magnetic Materials
Authors
, , , , ,