Fatigue-free Bi3.2Nd0.8Ti3O12 ferroelectric thin films were successfully prepared on p-Si(1 1 1) substrate using chemical solution deposition process. The orientation and formation of thin film under different annealing schedules were studied. XRD analysis indicated that (2 0 0)-oriented films with degree of orientation of I(2 0 0)/I(1 1 7) = 2.097 and 0.466 were obtained by preannealing for 10 min at 400 °C followed by rapid thermal annealing for 3, 10 and 20 min at 700 °C, respectively, (0 0 8)-oriented films with degree of orientation of I(0 0 8)/I(1 1 7) = 1.706 were obtained by rapid thermal annealing for 3 min at 700 °C without preannealing, and (0 0 8)-oriented films with degree of orientation of I(0 0 8)/I(1 1 7) = 0.719 were obtained by preheating the film from room temperature at 20 °C/min followed by annealing for 10 min at 700 °C. The a-axis and c-axis orientation decreased as increase of annealing time due to effects of (1 1 1)-oriented substrate. AFM analysis further indicated that preannealing at 400 °C for 10 min followed by rapid thermal annealing for 3 min at 700 °C resulted in formation of platelike crystallite parallel to substrate surface, however rapid thermal annealing for 3 min at 700 °C without preannealing resulted in columnar crystallite perpendicular to substrate surface.
Related Topics
Physical Sciences and Engineering
Materials Science
Electronic, Optical and Magnetic Materials
Authors
H.Y. He, J.F. Huang, L.Y. Cao, L.S. Wang,