Abstract
This paper reported the synthesis, crystal structure and electrical conductivity properties of Ni-doped ZnO powders (i.e. Zn1-X NiXO binary system, X =0, 0.0025, 0.005, 0.0075 and in the range 0.01â¤Xâ¤0.15). I-phase samples, which were indexed as single phase with a hexagonal (wurtzite) structure in the Zn1-X NiXO binary system, were determined by X-ray diffraction (XRD). The widest range of the I-phase was determined as 0â¤Xâ¤0.03 at 1200°C; above this range the mixed phase was observed. The impurity phase was determined as NiO when compared with standard XRD data, using the PDF program. We focused on single I-phase ZnO samples which were synthesized at 1200°C because of the widest range of solubility limit at this temperature. It was observed that the lattice parameters a and c of the I-phase decreased with Ni doping concentration. The morphology of the I-phase samples was analyzed with a scanning electron microscope. The electrical conductivity of the pure ZnO and single I-phase samples were studied by using the four-probe dc method at temperatures between 100 and 950°C in air atmosphere. The electrical conductivity values of pure ZnO and 3 mol% Ni-doped ZnO samples at 100°C were 2Ã10â6 and 4.8Ã10â6 Ωâ1 cmâ1, and at 950°C they were 1.8 and 3.6 Ωâ1 cmâ1, respectively. In other words, electrical conductivity increased with Ni doping concentration.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Chemistry
Authors
Hakan Ãolak, Orhan TürkoÄlu,