Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1556782 | Journal of Materials Science & Technology | 2011 | 6 Pages |
Abstract
β-tricalcium phosphate (β-TCP) powder and Na2O-CaO-MgO-P2O5 glass binder were synthesized and mixed, and then the biodegradable porous calcium phosphate ceramics were successfully prepared by foaming and sintering at 850°C. The as-prepared ceramics possess a high porosity with partial three-dimension interconnected macro- and micro-pores. As in vitro experiment testified, the calcium phosphate ceramics (CPCs) has good degradability.
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Chemistry
Authors
Honglian Dai, Xinyu Wang, Yinchao Han, Xin Jiang, Shipu Li,