Abstract
⺠0.5 wt% hydrogen is added to Ti-6Al-4V alloy, donated as Ti-6Al-4V-0.5 H alloy. ⺠Ti-6Al-4V-0.5 H alloy was friction stir welded using a W-Re pin tool. ⺠Hydrogen was removed from the as-welded joint by post-weld dehydrogenation. ⺠The effect of 0.5 wt% hydrogen addition on microstructural evolution is revealed.