Defect bands following the casting contour are often observed in high-pressure die cast (HPDC) components. In this article, suitable methods for measuring the thickness (w) and grain size in the bands (dsb) in HPDCs have been developed. The w/dsb relationship of defect bands has been investigated in HPDC specimens from a range of alloys, casting geometries and band locations within castings. Samples include aluminum alloy, AlSi4MgMn and AlMg5Si2Mn, tensile test bars cast by cold-chamber (cc) HPDC and a magnesium alloy, AM50, hot-chamber (hc) HPDC steering-wheel component. The band thicknesses were measured to be in the range 7–18 mean grains wide. This is substantial evidence that defect bands form due to strain localization in partially solidified alloys during cc and hc HPDC. Additionally, within this range, the w/dsb ratio decreases with increasing distance from the casting center in a cross-section containing multiple bands.

Related Topics
Physical Sciences and Engineering Materials Science Materials Science (General)
Authors
, , , ,